Technical Data
| Item |
LGM-80 |
| Al2O3 %≥ |
78 |
| Fe2O3 % ≤ |
1.0 |
| Apparent porosity % ≤ |
18 |
| Bulk density(g/cm3)≥ |
2.65 |
| Cold crush strength Mpa ≥ |
80 |
| 0.2 Mpa refractoriness under load (℃)≥ |
1700 |
| Thermal expansion(1000℃)% < |
0.6 |
| Refractoriness(℃)≥ |
1790 |
| Thermal shock resistance(1100℃,water)cycles > |
30 |
|