| Silica Refractory Bricks For Coke Oven |
Technical Data
| Item |
bottom,wall |
other |
| SiO2 %≥ |
94.5 |
94.5 |
| Al2O3 %≤ |
1.5 |
1.5 |
| Fe2O3 %≤ |
1.5 |
1.5 |
| CaO %≤ |
1.5 |
1.5 |
| Apparent porosity % ≤ |
22 |
24 |
| True density g/cm3 ≤ |
2.33 |
2.34 |
| Thermal expansion(1000℃)% ≤ |
1.28 |
1.30 |
| Linear change after reheating(1450℃×2h),% |
0~ +0.2 |
0 |
| 0.2mpa refractoriness under load ,℃≥ |
1650 |
1650 |
| Residual quartz % ≤ |
1.0 |
1.0 |
|